PS (SB) electrically conductive
(virgin material, regrind or reworking)
increased impact-modified
adjustment from 103 – 107 Ohm/cm2
individual adjustments of conductivity by agreement
ABS electrically conductive
(virgin material)
PS/PE-Blend electrically conductive
adjustments from 104 – 106 Ohm/cm2 TPE-EL / PS (SB)-EL – Co-extrusion
PS (SB) electrically conductive with a top coat of TPE electrically conductive
(TPE-EL also available on both sides)
TPE-EL / PS/PE-Blend-EL – Co-extrusion
(PS/PE-Blend electrically conductive with a top coat
TPE electrically conductive
TPE-EL also available on both sides)
TPU-EL / ABS-EL – Co-extrusion
(ABS electrically conductive with a top coat
TPE electrically conductive
(TPU-EL also available on both sides)
PS (SB) ESD-Nano-Tube
extended adjustment range of the electrically
conductive resistance (102 – 1010 Ohm)
low material abrasion
homogeneous electrostatic properties
no pre-drying necessary
no moisture absorption during storage periods
low loss of conductivity during thermoforming
good forming properties = reduced cycle times
excellent surface qualities
low specific gravity
good impact strength